 RP grade 75-150 мм
 RP grade 200-350 мм
 RP grade 400-600 мм
 RP grade 700
HP grade 200-400мм
HP grade 450-700 мм
UHP grade 200-400 мм
UHP grade 450-700 мм
  • Bulk density (no less), g/cm3 Electrode RP Grade 1,6
  • Bulk density (no less), g/cm3 Nipple RP Grade
  • Ash content (no more), % Electrode RP Grade 0,5
  • Ash content (no more), % Nipple RP Grade
  • Electrical resistivity (no more), µOhm•m Electrode RP Grade 7,2
  • Electrical resistivity (no more), µOhm•m Nipple RP Grade
  • Thermal expansion coefficient, 100-600 °C (no more), 10-6•1/°С Electrode RP Grade 2,8
  • Thermal expansion coefficient, 100-600 °C (no more), 10-6•1/°С Nipple RP Grade
  • Bending strength (no less), MPa Electrode RP Grade 10,5
  • Bending strength (no less), MPa Nipple RP Grade
  • Elastic modulus (no more), GPa Electrode RP Grade 9,3
  • Elastic modulus (no more), GPa Nipple RP Grade
  • Bulk density (no less), g/cm3 Electrode RP Grade 1,55
  • Bulk density (no less), g/cm3 Nipple RP Grade
  • Ash content (no more), % Electrode RP Grade 0,5
  • Ash content (no more), % Nipple RP Grade
  • Electrical resistivity (no more), µOhm•m Electrode RP Grade 7,5
  • Electrical resistivity (no more), µOhm•m Nipple RP Grade
  • Thermal expansion coefficient, 100-600 °C (no more), 10-6•1/°С Electrode RP Grade 2,8
  • Thermal expansion coefficient, 100-600 °C (no more), 10-6•1/°С Nipple RP Grade
  • Bending strength (no less), MPa Electrode RP Grade 10,5
  • Bending strength (no less), MPa Nipple RP Grade
  • Elastic modulus (no more), GPa Electrode RP Grade 9,3
  • Elastic modulus (no more), GPa Nipple RP Grade
  • Bulk density (no less), g/cm3 Electrode RP Grade 1,55
  • Bulk density (no less), g/cm3 Nipple RP Grade
  • Ash content (no more), % Electrode RP Grade 0,5
  • Ash content (no more), % Nipple RP Grade
  • Electrical resistivity (no more), µOhm•m Electrode RP Grade 8
  • Electrical resistivity (no more), µOhm•m Nipple RP Grade
  • Thermal expansion coefficient, 100-600 °C (no more), 10-6•1/°С Electrode RP Grade 2,8
  • Thermal expansion coefficient, 100-600 °C (no more), 10-6•1/°С Nipple RP Grade
  • Bending strength (no less), MPa Electrode RP Grade 8,4
  • Bending strength (no less), MPa Nipple RP Grade
  • Elastic modulus (no more), GPa Electrode RP Grade 9,3
  • Elastic modulus (no more), GPa Nipple RP Grade
  • Bulk density (no less), g/cm3 Electrode RP Grade 1,55
  • Bulk density (no less), g/cm3 Nipple RP Grade
  • Ash content (no more), % Electrode RP Grade 0,5
  • Ash content (no more), % Nipple RP Grade
  • Electrical resistivity (no more), µOhm•m Electrode RP Grade 8,5
  • Electrical resistivity (no more), µOhm•m Nipple RP Grade
  • Thermal expansion coefficient, 100-600 °C (no more), 10-6•1/°С Electrode RP Grade 2,8
  • Thermal expansion coefficient, 100-600 °C (no more), 10-6•1/°С Nipple RP Grade
  • Bending strength (no less), MPa Electrode RP Grade 8,4
  • Bending strength (no less), MPa Nipple RP Grade
  • Elastic modulus (no more), GPa Electrode RP Grade 9,3
  • Elastic modulus (no more), GPa Nipple RP Grade
  • Bulk density (no less), g/cm3 Electrode HP Grade 1,68
  • Bulk density (no less), g/cm3 Nipple HP Grade 1,74
  • Ash content (no more), % Electrode HP Grade 0,3
  • Ash content (no more), % Nipple HP Grade 0,3
  • Electrical resistivity (no more), µOhm•m Electrode HP Grade 6,8
  • Electrical resistivity (no more), µOhm•m Nipple HP Grade 6,2
  • Thermal expansion coefficient, 100-600 °C (no more), 10-6•1/°С Electrode HP Grade 2,3
  • Thermal expansion coefficient, 100-600 °C (no more), 10-6•1/°С Nipple HP Grade 2,1
  • Bending strength (no less), MPa Electrode HP Grade 10,5
  • Bending strength (no less), MPa Nipple HP Grade 15
  • Elastic modulus (no more), GPa Electrode HP Grade 12
  • Elastic modulus (no more), GPa Nipple HP Grade 16
  • Bulk density (no less), g/cm3 Electrode HP Grade 1,65
  • Bulk density (no less), g/cm3 Nipple HP Grade 1,74
  • Ash content (no more), % Electrode HP Grade 0,3
  • Ash content (no more), % Nipple HP Grade 0,3
  • Electrical resistivity (no more), µOhm•m Electrode HP Grade 7,5
  • Electrical resistivity (no more), µOhm•m Nipple HP Grade 6,3
  • Thermal expansion coefficient, 100-600 °C (no more), 10-6•1/°С Electrode HP Grade 2,3
  • Thermal expansion coefficient, 100-600 °C (no more), 10-6•1/°С Nipple HP Grade 2,1
  • Bending strength (no less), MPa Electrode HP Grade 10,8
  • Bending strength (no less), MPa Nipple HP Grade 15
  • Elastic modulus (no more), GPa Electrode HP Grade 12
  • Elastic modulus (no more), GPa Nipple HP Grade 16
  • Bulk density (no less), g/cm3 Electrode UHP Grade 1,68
  • Bulk density (no less), g/cm3 Nipple UHP Grade 1,76
  • Ash content (no more), % Electrode UHP Grade 0,2
  • Ash content (no more), % Nipple UHP Grade 0,2
  • Electrical resistivity (no more), µOhm•m Electrode UHP Grade 6
  • Electrical resistivity (no more), µOhm•m Nipple UHP Grade 5
  • Thermal expansion coefficient, 100-600 °C (no more), 10-6•1/°С Electrode UHP Grade 1,4
  • Thermal expansion coefficient, 100-600 °C (no more), 10-6•1/°С Nipple UHP Grade 1,3
  • Bending strength (no less), MPa Electrode UHP Grade 11
  • Bending strength (no less), MPa Nipple UHP Grade 17
  • Elastic modulus (no more), GPa Electrode UHP Grade 14
  • Elastic modulus (no more), GPa Nipple UHP Grade 18
  • Bulk density (no less), g/cm3 Electrode UHP Grade 1,66
  • Bulk density (no less), g/cm3 Nipple UHP Grade 1,76
  • Ash content (no more), % Electrode UHP Grade 0,2
  • Ash content (no more), % Nipple UHP Grade 0,2
  • Electrical resistivity (no more), µOhm•m Electrode UHP Grade 6,5
  • Electrical resistivity (no more), µOhm•m Nipple UHP Grade 5,5
  • Thermal expansion coefficient, 100-600 °C (no more), 10-6•1/°С Electrode UHP Grade 1,4
  • Thermal expansion coefficient, 100-600 °C (no more), 10-6•1/°С Nipple UHP Grade 1,3
  • Bending strength (no less), MPa Electrode UHP Grade 10,5
  • Bending strength (no less), MPa Nipple UHP Grade 17
  • Elastic modulus (no more), GPa Electrode UHP Grade 14
  • Elastic modulus (no more), GPa Nipple UHP Grade 18
Order Electrodes graphitized
Description
Specifications

Electrodes graphitized is a carbon-containing material with excellent performance characteristics:
• easily gives in to mechanical processing;
• features uniform structure, low porosity, smooth surface, high strength and electrical conductivity;
• resistant to acids and moisture;
• practically does not oxidize.

Scope of Electrodes graphitized:
• iron and steel smelting;
• production of building materials;
• production of paint coatings;
• production of special grades of glass, anti-friction plastics, etc.

We would like to offer such brands of Electrodes graphitized at affordable price with delivery worldwide:
FC-1. The carbon content is not less than 97%, the mass fraction of moisture is not more than 1%, the ash content is not more than 2%, the sulfur content is not more than 1%, the concentration of volatile compounds is not more than 1%.
FC-2. The carbon content is not less than 99%, the mass fraction of moisture is not more than 1%, the ash content is not more than 1%, the sulfur content is not more than 0.05%, the concentration of volatile compounds is not more than 1%.
FC-3. The carbon content is not less than 95%, the mass fraction of moisture is not more than 1%, the ash content is not more than 5%, the sulfur content is not more than 0.5%, the concentration of volatile compounds is not more than 1%.

Quality indicators can be coordinated by request.
To get detailed information, get acquainted with the physical and chemical characteristics of a particular product and make an order, please contact us via messangers or fill the request in.
The ELMAR Company produces any fraction with any parameters needed.
Big bag packaging or bulk.

We are looking forward to hearing from you soon!

Coal prices including VAT

Our other products